They may need to move on to subsequent test shots as they refine the tool. Each step takes a few weeks, so the
|
||||
fewer test shots you need the better. Factories are getting pretty good now in that most of the ones I've worked
|
||||
with get it right on the first or second try. After they're happy with the tool, they harden it, which means it's
|
||||
good for about 100,000 shots before it needs to be refinished.
|
||||
good for about 100,000 shots before it needs to be refinished. This process usually involves picking a texture,
|
||||
which is usally done out of a book. Textures are easy to add, and can cover up many manufacturing defects.
|
||||