From 67968add7b07ae626b2d0285083312cfed123594 Mon Sep 17 00:00:00 2001 From: Sean Cross Date: Mon, 21 Jan 2019 08:28:11 +1300 Subject: [PATCH] finishing: annotate moldtech stuff Signed-off-by: Sean Cross --- index.html | 3 ++- 1 file changed, 2 insertions(+), 1 deletion(-) diff --git a/index.html b/index.html index b264300..fe7df08 100644 --- a/index.html +++ b/index.html @@ -754,7 +754,8 @@ They may need to move on to subsequent test shots as they refine the tool. Each step takes a few weeks, so the fewer test shots you need the better. Factories are getting pretty good now in that most of the ones I've worked with get it right on the first or second try. After they're happy with the tool, they harden it, which means it's - good for about 100,000 shots before it needs to be refinished. + good for about 100,000 shots before it needs to be refinished. This process usually involves picking a texture, + which is usally done out of a book. Textures are easy to add, and can cover up many manufacturing defects.